25.9.2026

How to reduce pipeline wear in the pneumatic transport of minerals?

Corrosion in pipelines is one of the most expensive problems in pneumatic material handling. Minerals are often hard, abrasive and irregularly shaped, which effectively wears out the pipeline, especially in bends, branches and at points of speed change. Uncontrolled wear leads to unexpected downtime, increasing maintenance costs and ultimately to the premature replacement of the entire system.

In this guide, we will go through four concrete steps that will help you reduce pipeline wear in pneumatic conveying of minerals. The steps cover identifying the root causes of wear, optimizing flow rate, material selection, and predictive monitoring. Discover our pneumatic conveying solutions and see what options are available for demanding conditions.

Identify the factors causing wear in your pipeline

Before you can reduce wear and tear, you need to understand where it occurs and why. Pipe wear is not uniform, but rather concentrated in specific critical points. By identifying these points, you can target your actions correctly and avoid unnecessary resource consumption.

Wear is caused by three main factors: the hardness and particle size of the material, the flow rate, and the geometry of the piping system. Hard, angular mineral particles, such as quartz or grit, wear the steel surface much faster than round and softer materials. High flow rate accelerates wear exponentially, not linearly.

Check the following risks in your plumbing system:

  • Curves and corners, especially 90-degree turns
  • Pipe sections and distribution pieces
  • Feed points where material meets the flow
  • Horizontal to vertical transitions
  • Points where the flow speed changes rapidly

Once you have identified the risk areas, document them systematically. This mapping serves as the basis for all the steps in the following phases and makes monitoring systematic.

Optimize the flow rate and pressure method

Flow rate is the single most significant factor in pipeline wear. Research and practical experience show that wear increases with the second or even the third power of the flow rate. This means that halving the flow rate can reduce wear by up to 75 percent.

Pneumatic transport uses two main transfer methods: dilute phase conveying and dense phase conveying. In dilute phase conveying, material moves through the pipeline at a high air speed, typically 15 meters per second or more. This is a simple and cost-effective method, but with abrasive minerals it consumes the pipeline quickly. In dense phase conveying, material moves more slowly as a ”cone” at a lower speed, usually between 7 and 10 meters per second. A lower speed directly means less wear.

Optimise the flow rate in practice as follows:

  1. Determine the minimum flow rate of your material, i.e. the minimum speed at which the material still moves through the pipeline without clogging.
  2. Set the operating speed as close as possible to this minimum, but leave a sufficient safety margin for process disruptions.
  3. Consider switching to a roller conveyor if your material's characteristics allow it. Roller conveyors are particularly suitable for coarse, abrasive minerals.
  4. Ensure that the pressure is uniform throughout the entire transport period. Variations in pressure cause speed spikes, which accelerate wear locally.

After optimizing the flow rate, you should have a clear understanding of whether your system operates as a jet flow or a slug flow, and whether a transition to a lower-speed method is possible. Contact us, If you want an expert assessment of the optimization possibilities for your own system.

Choose the right materials and piping geometry

Optimizing the flow rate significantly reduces wear, but that is not enough on its own when dealing with particularly abrasive minerals. The material and geometric choices of the piping determine how long the piping will last in practice.

In the selection of piping material, carbon steel is rarely the best option for demanding mineral transport. Wear-resistant steels, such as Hardox-type materials, withstand wear many times better than conventional structural steel. Alternatively, pipes equipped with a ceramic lining can be used especially at the most critical wear points. The ceramic lining is a more expensive investment, but the service life can be significantly longer with abrasive materials.

Regarding geometry, do the following:

  1. Represents sharp 90-degree bends with long radius bends. The recommended radius of the bend is at least 5 times the diameter of the pipe, preferably more.
  2. Use consumption-protected specialty bushings at critical turning points. So-called ”back pressure” or ”T-routes” disperse wear over a wider area.
  3. Design the piping route so that there are as few bends as possible. Every bend is a potential point of wear.
  4. Make sure that the diameter of the pipeline is properly sized. A diameter that is too small will force you to increase the speed, while a diameter that is too large can cause material to fall and cause uneven flow.

The right piping material and carefully considered geometry can double or even triple the lifespan of the piping without any changes to the process. This is an investment that quickly pays off in reduced downtime and maintenance costs. View our case studies and see how these solutions have been implemented in practical settings in demanding process environments.

Track wear and predict maintenance needs

The measures in the previous stages significantly reduce wear but do not completely eliminate it. Systematic monitoring is the only way to ensure that the pipeline remains operational and that maintenance measures are carried out at the right time, before wear causes an unexpected shutdown.

Several methods are used in wear monitoring. The simplest is a regular visual inspection combined with wall thickness measurements using an ultrasonic meter. It is advisable to focus the measurements specifically on the critical points identified in the first phase. In more advanced systems, continuous sensor-based monitoring solutions can be used that alert when the wall thickness approaches the critical limit.

Construct a proactive maintenance program as follows:

  1. Set an alarm limit for each critical pipe section, for example 30 percent of the original wall thickness, whereby part is replaced before the rupture occurs.
  2. Schedule regular measurement rounds based on the process’s usage hours or calendar period, depending on which comes first.
  3. Keep track of the wear history for each measurement point. The history data reveals the wear rate trends and helps predict the timing of the next replacement.
  4. Keep the most common wear parts in stock, such as bushings and special parts. Fast replacement minimizes downtime.

When monitoring is systematic and historical data is collected, you can predict maintenance needs weeks or months in advance. This transforms reactive repairs into planned maintenance, which is both more efficient from a production standpoint and more cost-effective.

The management of pipeline wear is an ongoing process, not a one-time project. By identifying the factors that cause wear, optimizing the flow rate, making the right material and geometric choices, and monitoring wear systematically, you can significantly extend the life of the pipeline and maintain high operational reliability of production. Kopar has designed and supplied pneumatic conveying systems for demanding mineral processing processes for nearly 50 years. Discover our pneumatic conveying solutions or Get in touch, So, let’s go through how we can help you reduce pipeline wear in your own process. You can also find more information about solutions suitable for different material types in the article. what is the best pneumatic conveyor for fine materials.

Kopar Service Manager